Drying Settings (Blast Drying Oven) - 65 °C,8 h
Nozzle Temperature - 230 - 260 °C
Bed Temperature - 65 - 75 °C With Glue
Printing Speed - < 220 mm/s
Vicat Softening Temperature- 79 °C
Heat Deflection Temperature - 74 °C
Melting Temperature - 228 °C
Melt Index - 11.7 ± 1.5 g/10 min
Tensile Strength - 33 ± 4 MPa
Breaking Elongation Rate - 8.2 ± 1.3 %
Bending Modulus - 1610 ± 130 MPa
Bending Strength - 68 ± 3 MPa
Impact Strength- 37.4 ± 3.3 kJ/m²